By comparison of the experimental image in Fig. 7 with the
modeling data in Fig. 8 and assuming significant averaging
due to the small lateral island size as compared to the HRTEM foil
(∼15 nm), one may conclude that the actual CdSe composition of
SML islands is at or higher than 40% and the adatom-induced
“wetting layer” composition is 15–20% or lower. .